Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-23 UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal pr.. |
|||
Charpy Impact, Notched | 0.750 J/cm² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Charpy Impact, Notched | 0.750 J/cm² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179 |
GEHR Plastics POM-ELS Acetal, Electrically Conductive Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Charpy Impact, Notched | 0.750 J/cm² @Temperature -20.0 °C |
3.57 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
IRPC Polimaxx Polene 2346NC Polypropylene Block Copolymer CHARACTERISTICS: HIGH STIFFNESS, HIGH IMPACT, MEDIUM FLOW, HEAT STABILITY CONTAIN ANTISTATIC AND UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene G2855 High Density Polyethylene CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
LATI Laticonther 92 GR/65 PUR, 65% Graphite Reinforced High thermal conductivity product based on Polyurethane (PUR). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
LATI Latistat 67-08 PA66, Impact Modified Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, Conditioned Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | IS0179 |
Zhejiang Juner 302-G20 20% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced PEEK-GF30Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBATER BFA15 PBT, 15% glass fiber reinforced, flame retardant PBT-GF15 FRInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene J 683 Polypropylene Copolymer Copper ResistantInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | |
Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.I.. |
|||
Charpy Impact, Notched | 0.750 J/cm² | 3.57 ft-lb/in² | ISO 179/1eA |
Radici Radiflam® B RV 300 AE Polybutylene Terephthalate Raditer® B RV 300AE is a glass fiber reinforced, self-extinguishing UL-94 V-0 (with halogen) thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent therma.. |