Polymer Property : Charpy Impact, Notched = 14.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.100 - 3.10 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 14.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.690 J/cm² Grade Count:100
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.500 - 3.10 J/cm²
2.38 - 14.8 ft-lb/in²
Average value: 1.58 J/cm² Grade Count:31
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..