Polymer Property : Charpy Impact, Notched = 1.90 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.40 - 1.90 J/cm²
6.66 - 9.04 ft-lb/in²
Average value: 1.76 J/cm² Grade Count:5
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Charpy Impact, Notched 0.200 - 1.90 J/cm²

@Temperature -40.0 - -20.0 °C
0.952 - 9.04 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.924 J/cm² Grade Count:51
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Charpy Impact, Notched 0.350 - 1.90 J/cm²

@Temperature -40.0 - -30.0 °C
1.67 - 9.04 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.784 J/cm² Grade Count:15
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Charpy Impact, Notched 0.450 - 1.90 J/cm²

@Temperature -30.0 - -30.0 °C
2.14 - 9.04 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.16 J/cm² Grade Count:54
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.400 - 1.90 J/cm²

@Temperature -30.0 - 30.0 °C
1.90 - 9.04 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.870 J/cm² Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
Copyright © lookpolymers.com All Rights Reserved