Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.89 J/cm² @Temperature 22.8 °C |
9.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Charpy Impact, Notched | 1.89 J/cm² @Temperature 22.8 °C |
9.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Charpy Impact, Notched | 1.89 J/cm² @Temperature 22.8 °C |
9.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Charpy Impact, Notched | 1.89 J/cm² @Temperature 22.8 °C |
9.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Charpy Impact, Notched | 1.89 J/cm² @Temperature 22.8 °C |
9.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Charpy Impact, Notched | 1.89 J/cm² @Temperature 22.8 °C |
9.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |