Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 22.0 MPa @Strain 1.00 % |
3190 psi @Strain 1.00 % |
dry; ISO 604 |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Compressive Yield Strength | 22.0 MPa @Strain 1.00 % |
3190 psi @Strain 1.00 % |
dry; ISO 604 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Compressive Yield Strength | 22.0 MPa @Strain 1.00 % |
3190 psi @Strain 1.00 % |
dry; ISO 604 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Compressive Yield Strength | 22.0 MPa @Strain 6.00 %, Temperature 316 °C |
3190 psi @Strain 6.00 %, Temperature 601 °F |
ASTM D695 Modified |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |