Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0689 - 0.117 MPa @Strain 25.0 % |
10.0 - 17.0 psi @Strain 25.0 % |
Range, 0.2"/min. strain rate |
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Compressive Yield Strength | 0.0689 MPa @Strain 8.00 % |
10.0 psi @Strain 8.00 % |
Load applied normal to fiber plane |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Compressive Yield Strength | 0.0689 MPa @Strain 3.00 % |
10.0 psi @Strain 3.00 % |
Load applied normal to fiber plane |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Compressive Yield Strength | 0.0690 MPa @Strain 25.0 % |
10.0 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.0690 MPa @Strain 10.0 % |
10.0 psi @Strain 10.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.0689 MPa @Strain 2.00 % |
10.0 psi @Strain 2.00 % |
Load applied parallel to fiber plane |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |