Polymer Property : Ball Indentation Hardness = 23.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 23.0 - 63.0 MPa
3340 - 9140 psi
Average value: 39.4 MPa Grade Count:14
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Ball Indentation Hardness 23.0 - 37.0 MPa
3340 - 5370 psi
Average value: 32.0 MPa Grade Count:9
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Ball Indentation Hardness 23.0 - 28.0 MPa
3340 - 4060 psi
DIN 53 456
Isoflon FEP Fluorinated Ethylene Propylene
Fluoropolymer material specifications.Information provided by Isoflon.
Ball Indentation Hardness 23.0 - 28.0 MPa
3340 - 4060 psi
DIN 53 456
Isoflon PTFE Polytetrafluoroethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Ball Indentation Hardness 23.0 MPa
3340 psi
132 N/10s; ISO 2039
Borealis Daplen™ EF005AE Polypropylene TPO Compound
Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
Ball Indentation Hardness >= 23.0 MPa
>= 3340 psi
ISO 2032
Adamas Adalon® 902 PTFE, 1% Conductive filler
Information provided by Adamas, HPM
Ball Indentation Hardness 23.0 - 90.0 MPa
3340 - 13100 psi
Average value: 49.3 MPa Grade Count:31
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..