Polymer Property : Ball Indentation Hardness = 4060 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 23.0 - 28.0 MPa
3340 - 4060 psi
DIN 53 456
Isoflon FEP Fluorinated Ethylene Propylene
Fluoropolymer material specifications.Information provided by Isoflon.
Ball Indentation Hardness 23.0 - 28.0 MPa
3340 - 4060 psi
DIN 53 456
Isoflon PTFE Polytetrafluoroethylene
Fluoropolymer material specifications.Information provided by Isoflon.