Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 23.0 - 37.0 MPa | 3340 - 5370 psi | Average value: 32.0 MPa Grade Count:9 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |