Ball Indentation Hardness 23.0 - 37.0 MPa
3340 - 5370 psi
Average value: 32.0 MPa Grade Count:9
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..