Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 25.0 J | 18.4 ft-lb | ASTM D3029 |
LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low foggingApplication.. |
|||
Gardner Impact | 25.0 - 35.0 J | 18.4 - 25.8 ft-lb | SABIC Method |
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East) NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r.. |
|||
Gardner Impact | 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
LyondellBasell Hifax™ ETA-3163UV Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, UV-stabilized thermoplastic olefin resin, excellent impact and stiffness balance, excellent weatherability, good processabilityApplications: mold.. |