LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low foggingApplications: automotive instrument panel components, knee bolsters and end caps, glove box doorsDescription: Hifax CB189FC medium melt flow, minearl-filled thermoplasstic olefin resin has a very good balance of impact, stiffness, dimensional stability and processability. It was designed specifically for use in various automotive interior trim components.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
Tool, Montell
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256A
Gardner Impact 25.0 J
18.4 ft-lb
ASTM D3029
19.0 J

@Temperature -30.0 °C
14.0 ft-lb

@Temperature -22.0 °F
ASTM D3029
Impact Test 15.0 J

@Temperature -30.0 °C
11.1 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ASTM D648