Mechanical Properties Metric English Comments
Gardner Impact 25.0 - 35.0 J
18.4 - 25.8 ft-lb
SABIC Method
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East)
NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r..