Mechanical Properties Metric English Comments
Gardner Impact 1.00 - 1.00 J

@Temperature -30.0 - -30.0 °C
0.738 - 0.738 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J Grade Count:1
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Gardner Impact 1.00 - 1.00 J

@Temperature -30.0 - -30.0 °C
0.738 - 0.738 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J Grade Count:1
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..