Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.90 - 1.90 J @Temperature -30.0 - -30.0 °C |
1.40 - 1.40 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 1.90 J Grade Count:1 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Puncture Energy | 1.90 - 1.90 J @Load <=91.8 kg |
1.40 - 1.40 ft-lb @Load <=202 lb |
Average value: 1.90 J Grade Count:1 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Puncture Energy | 1.90 J @Load <=81.6 kg, Temperature -30.0 °C |
1.40 ft-lb @Load <=180 lb, Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Puncture Energy | 1.90 J @Load <=91.8 kg, Temperature -30.0 °C |
1.40 ft-lb @Load <=202 lb, Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |