Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.20 GPa @Strain 2.88 %, Temperature 100 °C |
319 ksi @Strain 2.88 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Secant Modulus | 2.20 GPa @Strain 2.90 %, Temperature 0.000 °C |
319 ksi @Strain 2.90 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Secant Modulus | 2.20 GPa @Strain 1.02372 %, Temperature 100 °C |
319 ksi @Strain 1.02372 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |