Polymer Property : Secant Modulus = 2.20 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.20 GPa

@Strain 2.88 %,
Temperature 100 °C
319 ksi

@Strain 2.88 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7..
Secant Modulus 2.20 GPa

@Strain 2.90 %,
Temperature 0.000 °C
319 ksi

@Strain 2.90 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..
Secant Modulus 2.20 GPa

@Strain 1.02372 %,
Temperature 100 °C
319 ksi

@Strain 1.02372 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..