Mechanical Properties Metric English Comments
Secant Modulus 3.98 GPa

@Strain 2.59 %,
Temperature 23.0 °C
578 ksi

@Strain 2.59 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Secant Modulus 3.98 GPa

@Strain 0.690 %,
Temperature -40.0 °C
577 ksi

@Strain 0.690 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Secant Modulus 3.98 GPa

@Strain 0.690 %,
Temperature -40.0 °C
577 ksi

@Strain 0.690 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati..
Secant Modulus 3.98 GPa

@Strain 1.60 %,
Temperature 40.0 °C
577 ksi

@Strain 1.60 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti..