Mechanical Properties Metric English Comments
Secant Modulus 0.198 GPa

@Strain 4.87 %,
Temperature 100 °C
28.8 ksi

@Strain 4.87 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
Secant Modulus 0.199 GPa

@Strain 21.57 %,
Temperature 40.0 °C
28.8 ksi

@Strain 21.57 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers