Polymer Property : Secant Modulus = 0.198 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.198 GPa

@Strain 24.2 %,
Temperature 0.000 °C
28.6 ksi

@Strain 24.2 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
Secant Modulus 0.198 GPa

@Strain 4.87 %,
Temperature 100 °C
28.8 ksi

@Strain 4.87 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..