Secant Modulus 9.21 GPa

@Strain 1.20 %,
Temperature 23.0 °C
1340 ksi

@Strain 1.20 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Secant Modulus 9.23 GPa

@Strain 1.30 %,
Temperature 0.000 °C
1340 ksi

@Strain 1.30 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Secant Modulus 9.25 GPa

@Strain 2.70 %,
Temperature -40.0 °C
1340 ksi

@Strain 2.70 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per..
Secant Modulus 9.21 GPa

@Strain 1.20 %,
Temperature 23.0 °C
1340 ksi

@Strain 1.20 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..
Secant Modulus 9.23 GPa

@Strain 1.30 %,
Temperature 0.000 °C
1340 ksi

@Strain 1.30 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..
Secant Modulus 9.21 GPa

@Strain 0.786074 %,
Temperature 23.0 °C
1340 ksi

@Strain 0.786074 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..