Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 8.14 GPa

@Strain 0.110 %,
Temperature 0.000 °C
1180 ksi

@Strain 0.110 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Secant Modulus 8.12 GPa

@Strain 2.60 %,
Temperature -40.0 °C
1180 ksi

@Strain 2.60 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information..
Secant Modulus 8.15 GPa

@Strain 0.520 %,
Temperature 40.0 °C
1180 ksi

@Strain 0.520 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol..
Secant Modulus 8.11 GPa

@Strain 1.26111 %,
Temperature 23.0 °C
1180 ksi

@Strain 1.26111 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..