Mechanical Properties Metric English Comments
Secant Modulus 1.13 GPa

@Strain 1.27 %,
Temperature 40.0 °C
164 ksi

@Strain 1.27 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Secant Modulus 1.13 GPa

@Strain 1.27 %,
Temperature 40.0 °C
164 ksi

@Strain 1.27 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..
Secant Modulus 1.13 GPa

@Strain 0.150 %,
Temperature 40.0 °C
163 ksi

@Strain 0.150 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Secant Modulus 1.13 GPa

@Strain 5.40 %,
Temperature 23.0 °C
163 ksi

@Strain 5.40 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..