Mechanical Properties Metric English Comments
Compressive Yield Strength 0.600 MPa
87.0 psi
at 20% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane
TDI backbone: ester.Shore 00 Hardness: 90Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Compressive Yield Strength 0.600 MPa
87.0 psi
Sawbones Solid Rigid Polyurethane Foam 5 pcf Density
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech..