Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.600 MPa | 87.0 psi | at 20% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane TDI backbone: ester.Shore 00 Hardness: 90Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Compressive Yield Strength | 0.600 MPa | 87.0 psi | |
Sawbones Solid Rigid Polyurethane Foam 5 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |