Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.00700 - 0.0350 MPa | 1.02 - 5.08 psi | at 25% deflection; 0.2"/min strain rate |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Compressive Yield Strength | 0.0150 - 0.0350 MPa | 2.18 - 5.08 psi | 25% Compression |
BIW ASTM Class 2D1 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |