Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | <= 0.0150 MPa | <= 2.18 psi | 25% Compression |
BIW ASTM Class 2D0 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |
|||
Compressive Yield Strength | 0.0150 - 0.0350 MPa | 2.18 - 5.08 psi | 25% Compression |
BIW ASTM Class 2D1 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |