Polymer Property : Compressive Yield Strength = 2.18 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength <= 0.0150 MPa
<= 2.18 psi
25% Compression
BIW ASTM Class 2D0 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...
Compressive Yield Strength 0.0150 - 0.0350 MPa
2.18 - 5.08 psi
25% Compression
BIW ASTM Class 2D1 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...