Compressive Yield Strength 0.00700 - 0.0350 MPa
1.02 - 5.08 psi
at 25% deflection; 0.2"/min strain rate
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..