Mechanical Properties Metric English Comments
Compressive Yield Strength 117 - 269 MPa
17000 - 39000 psi
Average value: 151 MPa Grade Count:8
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim..