Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0138 - 0.0689 MPa @Strain 25.0 % |
2.00 - 10.0 psi @Strain 25.0 % |
0.2"/min. strain rate |
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade Thickness: 0.125"- 0.500"Color: BlackInformation provided by Rogers Corporation. |
|||
Compressive Yield Strength | 0.0138 MPa @Strain 25.0 % |
2.00 psi @Strain 25.0 % |
0.2"/min. strain rate |
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Compressive Yield Strength | 0.0138 MPa | 2.00 psi | at 1% Comp., RT, Parallel to Thickness |
Zircar Ceramics Z-MAG/2300 Soluble Fiber Insulation ZIRCAR NON-RCF Insulation Type Z-MAG/2300 is a rigid combination of soluble NON-RCF silica magnesia glass fibers and inorganic binder. It is suitable for use as a substitute for insulation containin.. |