Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0138 - 0.0689 MPa @Strain 25.0 % |
2.00 - 10.0 psi @Strain 25.0 % |
0.2"/min. strain rate |
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade Thickness: 0.125"- 0.500"Color: BlackInformation provided by Rogers Corporation. |
|||
Compressive Yield Strength | 0.0345 - 0.0689 MPa | 5.00 - 10.0 psi | TM R050-38 |
Resinlab® UR3001HP Black Urethane Encapsulant Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e.. |
|||
Compressive Yield Strength | 0.0345 - 0.0689 MPa | 5.00 - 10.0 psi | TM R050-38 |
Resinlab® UR3001HP Clear Urethane Encapsulant Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e.. |