Polymer Property : Compressive Yield Strength = 10.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0138 - 0.0689 MPa

@Strain 25.0 %
2.00 - 10.0 psi

@Strain 25.0 %
0.2"/min. strain rate
Rogers Corporation Poron® Shock Seal™ 4790-79-15 Urethane Foam, Industrial Grade
Thickness: 0.125"- 0.500"Color: BlackInformation provided by Rogers Corporation.
Compressive Yield Strength 0.0345 - 0.0689 MPa
5.00 - 10.0 psi
TM R050-38
Resinlab® UR3001HP Black Urethane Encapsulant
Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e..
Compressive Yield Strength 0.0345 - 0.0689 MPa
5.00 - 10.0 psi
TM R050-38
Resinlab® UR3001HP Clear Urethane Encapsulant
Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e..