Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0900 - 10.9 MPa | 13.1 - 1580 psi | Average value: 0.920 MPa Grade Count:56 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Compressive Yield Strength | 0.0900 MPa | 13.1 psi | at 20% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane MDI backbone: ether.Shore 00 Hardness: 60Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Compressive Yield Strength | 0.0900 MPa @Strain 25.0 % |
13.1 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Evacell EVA 100 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Compressive Yield Strength | 0.0900 MPa @Strain 50.0 % |
13.1 psi @Strain 50.0 % |
ASTM 1056/85 |
Eurofoam Siliconcell SIL 411 Silicone Foam Sheet Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Compressive Yield Strength | 0.0900 MPa | 13.1 psi | Compressive Load Deflection at 5%; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2350 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Compressive Yield Strength | 0.0900 MPa | 13.1 psi | Compressive Load Deflection at 5%; ASTM D575 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2375 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Compressive Yield Strength | 0.0900 - 2.33 MPa | 13.1 - 338 psi | Average value: 0.661 MPa Grade Count:10 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Compressive Yield Strength | 0.0900 - 0.159 MPa | 13.1 - 23.1 psi | at 25% deflection; 0.2"/min strain rate |
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Compressive Yield Strength | 0.0900 - 0.120 MPa | 13.1 - 17.4 psi | 25% Compression |
BIW ASTM Class 2D4 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |