Eurofoam Siliconcell SIL 411 Silicone Foam Sheet

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer Eurofoam s.r.l.
Trade Name Siliconcell
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Siliconcell SIL 411 Silicone Foam Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.210 - 0.290 g/cc
0.00759 - 0.0105 lb/in³
ISO 845-88
Mechanical Properties Metric English Comments
Hardness, Shore OO 40 - 50
40 - 50
ASTM D 2240
Tensile Strength 0.110 MPa
16.0 psi
ASTM D 412
Elongation at Break >= 200 %
>= 200 %
ASTM D 412
Compressive Yield Strength 0.0900 MPa

@Strain 50.0 %
13.1 psi

@Strain 50.0 %
ASTM 1056/85
Compression Set 15 %

@Strain 50.0 %
15 %

@Strain 50.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
ASTM D 3575
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Closed
Color White, Red
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Fire Resistance MV22 302
Pass