Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mearthane Products Corporation (MPC)
Trade Name Durethane™ M
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MDI backbone: ether.Shore 00 Hardness: 60Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Durethane M is very economical, and has excellent resistance to compression set. It can be formulated to form an integral skin.Applications: The compression set resistance of Durethane M makes it an effective material for applications with repeated compression cycles, such as actuator pads on postal meters and idler belts.Conductivity: All Durethane elastomers can be formulated to be electrically conductive, for applications involving electrostatic dissipation (ESD). Mearthane's proprietary conductivity process does not comprise the material performance specification of the urethane.Information provided by Mearthane Products Corporation.
Physical Properties Metric English Comments
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574A
Mechanical Properties Metric English Comments
Hardness, Shore A 15
15
ASTM D2240
Tensile Strength, Ultimate 7.60 MPa
1100 psi
ASTM D3574E
Elongation at Break 360 %
360 %
ASTM 3457E
100% Modulus 0.000303 GPa
0.0439 ksi
ASTM D3574E
200% Modulus 0.000660 GPa
0.0957 ksi
ASTM D3574E
Compressive Yield Strength 0.0600 MPa
8.70 psi
at 10% deflection; ASTM D3574C
0.0900 MPa
13.1 psi
at 20% deflection; ASTM D3574C
0.120 MPa
17.4 psi
at 30% deflection; ASTM D3574C
Resilience 49
49
Bashore Rebound; ASTM 2632D
Tear Strength Test 35
35
lb; Die C; ASTM 3457F