Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0900 - 10.9 MPa
13.1 - 1580 psi
Average value: 0.920 MPa Grade Count:56
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Compressive Yield Strength 0.0900 MPa
13.1 psi
at 20% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane
MDI backbone: ether.Shore 00 Hardness: 60Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
Compressive Yield Strength 0.0900 MPa

@Strain 25.0 %
13.1 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Evacell EVA 100 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Compressive Yield Strength 0.0900 MPa

@Strain 50.0 %
13.1 psi

@Strain 50.0 %
ASTM 1056/85
Eurofoam Siliconcell SIL 411 Silicone Foam Sheet
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Compressive Yield Strength 0.0900 MPa
13.1 psi
Compressive Load Deflection at 5%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2350 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..
Compressive Yield Strength 0.0900 MPa
13.1 psi
Compressive Load Deflection at 5%; ASTM D575
Aearo E-A-R Specialty Composites VersaDamp™ V-2375 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..
Compressive Yield Strength 0.0900 - 2.33 MPa
13.1 - 338 psi
Average value: 0.661 MPa Grade Count:10
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..
Compressive Yield Strength 0.0900 - 0.159 MPa
13.1 - 23.1 psi
at 25% deflection; 0.2"/min strain rate
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Compressive Yield Strength 0.0900 - 0.120 MPa
13.1 - 17.4 psi
25% Compression
BIW ASTM Class 2D4 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...