Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 52.6 - 210 kN/m | 300 - 1200 pli | Average value: 124 kN/m Grade Count:18 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |