Polymer Property : Flexural Strength = 50.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 50.3 MPa
7300 psi
ASTM D790-95
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene
This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase.
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow  (Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Techmer ES HiFill FR® ABS GB10 FR 10% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 10% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Techmer ES HiFill® PA6 0177 B Barium Sulfate Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Techmer ES HiFill® PA6/6 0146 A Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Techmer ES HiFill® PA6/6 0164 A Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Techmer ES HiFill® PA6 0180 B Barium Sulfate Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Flexural Strength 50.3 MPa
7300 psi
chs 0.05 in/min; ASTM D790
Diamond Polymers Centrex® 825 Sheet Extrusion Grade
Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
Flexural Strength 50.3 MPa
7300 psi
chs 0.05 in/min; ASTM D790
Diamond Polymers SBS 2160 Clear Styrene Butadiene Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Strength 50.3 MPa
7300 psi
ASTM D-790
Axiall Suprel® SVA 9412 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu..
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled
Data provided by Adell Plastics, Inc.
Flexural Strength 50.3 MPa
7300 psi
ASTM D790
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet)