Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 274 MPa | 39700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 274 MPa | 39700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA LNP* THERMOCOMP* UFW49S is a compound based on Polyphthalamide resin containing 45% Glass Fiber, 20% Wollastonite. Added features of this material include: Heat Stabilized, Low Warpage. |
|||
Flexural Strength | 274 MPa | 39700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 274 MPa | 39700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 (Asia Pacific) LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 274 MPa | 39700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Strength | 274 MPa | 39700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA (Asia Pacific) LNP* Thermocomp* UFW49S is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized, Low Warpage. |
|||
Flexural Strength | 274 MPa | 39700 psi | ISO 178 |
LNP Thermocomp® UFM-3249 HS BK8-115 Polyphthalamide, Glass Mineral Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |