Polymer Property : Flexural Strength = 274 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 274 MPa
39700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 274 MPa
39700 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA
LNP* THERMOCOMP* UFW49S is a compound based on Polyphthalamide resin containing 45% Glass Fiber, 20% Wollastonite. Added features of this material include: Heat Stabilized, Low Warpage.
Flexural Strength 274 MPa
39700 psi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66
LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Strength 274 MPa
39700 psi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 (Asia Pacific)
LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Strength 274 MPa
39700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66
LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive.
Flexural Strength 274 MPa
39700 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA (Asia Pacific)
LNP* Thermocomp* UFW49S is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized, Low Warpage.
Flexural Strength 274 MPa
39700 psi
ISO 178
LNP Thermocomp® UFM-3249 HS BK8-115 Polyphthalamide, Glass Mineral Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..