Material Notes:
LNP* THERMOCOMP* UFW49S is a compound based on Polyphthalamide resin containing 45% Glass Fiber, 20% Wollastonite. Added features of this material include: Heat Stabilized, Low Warpage.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 192 MPa
27800 psi
ISO 527
Elongation at Break 1.1 %
1.1 %
ISO 527
Flexural Strength 274 MPa
39700 psi
ISO 178
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
9.44 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696