Polymer Property : Flexural Strength = 29000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 80.0 - 200 MPa
11600 - 29000 psi
Parallel to Plane
Goodfellow Carbon-Carbon Composite
Carbon Fiber - Carbon MatrixInformation provided by Goodfellow.
Flexural Strength 193 - 200 MPa
28000 - 29000 psi
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..