Carbon Fiber - Carbon MatrixInformation provided by Goodfellow.
Physical Properties Metric English Comments
Density 1.30 - 1.80 g/cc
0.0470 - 0.0650 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 10.0 MPa
<= 1450 psi
Transverse
40.0 - 70.0 MPa
5800 - 10200 psi
Longitudinal
Tensile Modulus 20.0 - 30.0 GPa
2900 - 4350 ksi
Parallel to Plane
Flexural Strength 80.0 - 200 MPa
11600 - 29000 psi
Parallel to Plane
Flexural Modulus 10.0 - 20.0 GPa
1450 - 2900 ksi
Parallel to Plane
Compressive Strength 60.0 - 150 MPa
8700 - 21800 psi
Perpendicular to Plane
120 - 200 MPa
17400 - 29000 psi
Parallel to Plane
Shear Strength 20.0 - 30.0 MPa
2900 - 4350 psi
in Plane
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 1.50 µm/m-°C

@Temperature 20.0 - 1000 °C
0.833 µin/in-°F

@Temperature 68.0 - 1830 °F
CTE, linear, Transverse to Flow 6.00 µm/m-°C

@Temperature 20.0 - 1000 °C
3.33 µin/in-°F

@Temperature 68.0 - 1830 °F
6.00 µm/m-°C

@Temperature 20.0 - 1000 °C
3.33 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 50.0 - 100 W/m-K
347 - 694 BTU-in/hr-ft²-°F
Perpendicular to Plane
250 - 300 W/m-K
1740 - 2080 BTU-in/hr-ft²-°F
Parallel to Plane
Electrical Properties Metric English Comments
Electrical Resistivity 0.00300 ohm-cm
0.00300 ohm-cm