PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer PolyOne Corporation
Trade Name Stat-Tech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 10.3 GPa
1490 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 159 MPa
23100 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.993 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C

@Thickness 6.35 mm
284 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
BKUL Listed; UL 94
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
ASTM D257
Processing Properties Metric English Comments
Rear Barrel Temperature 266 - 282 °C
511 - 540 °F
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Front Barrel Temperature 277 - 293 °C
531 - 559 °F
Mold Temperature 71.1 - 116 °C
160 - 241 °F
Descriptive Properties Value Comments
Features Electromagnetic Shielding (EMI)
ESD Protection
Flame Retardant
Radio Frequency Shielding (RFI)
Filler / Reinforcement Nickel-Coated Carbon Fiber
Forms Pellets
Generic Material ABS+PC
Generic Name Acrylonitrile Butadiene Styrene + PC (ABS+PC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Aerospace Applications
Business Equipment
Electrical Parts
Electrical/Electronic Applications
Housings