Asahi Kasei Thermylene® P-20FG-1740 20% Glass Fiber Reinforced, Medium Impact

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P-20FG-1740 20% Glass Fiber Reinforced, Medium Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 65.5 MPa
9500 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 87.6 MPa
12700 psi
ASTM D790
Flexural Modulus 3.24 GPa
470 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm
2.90 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm
11.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
291 °F
ASTM D648