Polymer Property : Tensile Stress = 8.47 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 8.47 MPa

@Strain 174.29 %,
Temperature 90.0 °C
1230 psi

@Strain 174.29 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.47 MPa

@Strain 71.79 %,
Temperature 100 °C
1230 psi

@Strain 71.79 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 8.47 MPa

@Strain 60.24 %,
Temperature 120 °C
1230 psi

@Strain 60.24 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.47 MPa

@Strain 0.230 %,
Temperature 150 °C
1230 psi

@Strain 0.230 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin..