Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1230 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 8.50 MPa

@Strain 100 %
1230 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ V 3050D-S0097 Thermoplastic Elastomer (TPE)
OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef..
Tensile Stress 8.51 MPa

@Strain 300 %,
Temperature 23.0 °C
1230 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE)
Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer..
Tensile Stress 8.48 MPa

@Strain 100 %
1230 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Stress 8.48 MPa

@Strain 100 %
1230 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-340-S Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 8.50 MPa

@Strain 1.60 %,
Temperature 90.0 °C
1230 psi

@Strain 1.60 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)  (Unverified Data**)
Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 8.47 MPa

@Strain 174.29 %,
Temperature 90.0 °C
1230 psi

@Strain 174.29 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.50 MPa

@Strain 249.44 %,
Temperature 120 °C
1230 psi

@Strain 249.44 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.45 MPa

@Strain 23.65 %,
Temperature 90.0 °C
1230 psi

@Strain 23.65 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 8.47 MPa

@Strain 71.79 %,
Temperature 100 °C
1230 psi

@Strain 71.79 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 8.47 MPa

@Strain 60.24 %,
Temperature 120 °C
1230 psi

@Strain 60.24 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 8.45 MPa

@Strain 108.54 %,
Temperature 100 °C
1230 psi

@Strain 108.54 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.50 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1230 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 8.47 MPa

@Strain 0.230 %,
Temperature 150 °C
1230 psi

@Strain 0.230 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin..
Tensile Stress 8.48 MPa

@Strain 0.100 %,
Temperature 150 °C
1230 psi

@Strain 0.100 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..
Tensile Stress 8.51 MPa

@Strain 35.0 %,
Temperature 100 °C
1230 psi

@Strain 35.0 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 8.50 MPa

@Strain 50.0 %
1230 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G4078 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 8.45 MPa

@Strain 6.00 %,
Temperature 23.0 °C
1230 psi

@Strain 6.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 8.50 - 11.5 MPa

@Strain 200 %
1230 - 1670 psi

@Strain 200 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...
Tensile Stress 8.50 - 11.5 MPa

@Strain 200 %
1230 - 1670 psi

@Strain 200 %
TM-019G
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc...
Tensile Stress >= 8.50 MPa

@Strain 100 %
>= 1230 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 290A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 8.50 MPa

@Strain 300 %
>= 1230 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 682A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Copyright © lookpolymers.com All Rights Reserved