Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 67.0 MPa @Strain 16.16 %, Temperature -20.0 °C |
9720 psi @Strain 16.16 %, Temperature -4.00 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 67.0 MPa @Strain 3.00 %, Temperature 40.0 °C |
9720 psi @Strain 3.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 67.0 MPa @Strain 16.2 %, Temperature -20.0 °C |
9720 psi @Strain 16.2 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 67.0 MPa @Strain 4.00 %, Temperature -20.0 °C |
9720 psi @Strain 4.00 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |