Polymer Property : Tensile Stress = 2550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 17.6 MPa

@Strain 19.8 %,
Temperature 90.0 °C
2550 psi

@Strain 19.8 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
Tensile Stress 17.6 MPa

@Strain 0.900 %,
Temperature 150 °C
2550 psi

@Strain 0.900 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..
Tensile Stress 17.6 MPa

@Strain 5.00 %,
Temperature 120 °C
2550 psi

@Strain 5.00 %,
Temperature 248 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Tensile Stress 17.6 MPa

@Strain 1.36 %,
Temperature 0.000 °C
2550 psi

@Strain 1.36 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 17.6 MPa

@Strain 0.400 %,
Temperature 90.0 °C
2550 psi

@Strain 0.400 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal..